Polyurethane Potting Adhesive KYROVIA 8436
- Two-component, weight ratio 100:40
-
Low viscosity, flame retardancy compliant with UL 94V-0
-
High-strength cured product with a glossy and smooth surface, excellent flame retardancy, thermal conductivity, and electrical insulation
-
Good electrical performance, waterproof and vibration-resistant properties, and superior low-temperature characteristics
-
Suitable for potting and protecting electronic products operating in humid and vibrating environments
Performance Parameters
| Component A | |
| Color: | Black |
| Viscosity: | 6000~8000 mPa·s |
| Component B | |
| Color: | Brownish Red |
| Viscosity: | 150~250 mPa·s |
| Mixing | |
| Mixing Ratio (Weight Ratio A:B): | 100:40 |
| Viscosity After Mixing: | 1000~1500 mPa·s |
| Working Time: | 10 min |
| Curing Time @25℃: | 24 h |
| Hardness After Curing (Shore A): | 60~70A |